Working time 6—8 min • casting ring can be placed into the furnace at final temperature (950 °C / 1742 °F) for speed preheating or preheated in stages overnight • used for all alloy groups • the high overall expansion provides precision of fit • long working times and a very creamy mixing consistency • castings with extremely smooth surfaces ensure uniform quality and exact reproduction of the pattern